| 品牌:上海宇韓鋁業(yè) | 規(guī)格:0.8-6.0 | 材質(zhì):5356 |
| 產(chǎn)地:上海,江蘇 |
使用及存放說(shuō)明:
1、產(chǎn)品拆封后,在保質(zhì)期內(nèi)你可以直接施焊,不需要任何焊前處理。產(chǎn)品出廠包裝密封條件下可保存二年以上,拆去包裝后在通常大氣環(huán)境下可保質(zhì)三個(gè)月;
2、產(chǎn)品應(yīng)置于通風(fēng)、干燥及酸、堿、油介質(zhì)隔離的地方存放;
3、產(chǎn)品在運(yùn)輸中應(yīng)避免摔撞和受潮,以免損壞焊絲盤(pán)和影響焊絲質(zhì)量;
4、焊絲拆去包裝后,建議在焊絲上方施加適當(dāng)?shù)姆缐m遮蓋物;
5、對(duì)于超過(guò)保質(zhì)期的焊絲,建議在焊前進(jìn)行焊絲表面清理;
6、焊接過(guò)程中的電弧會(huì)刺激你的眼睛,請(qǐng)注意保護(hù)。
標(biāo)準(zhǔn):GB/T 10858-2008
ER5356焊材化學(xué)成分指標(biāo)%:
Si··················<0.25
Fe··················<0.40
Cu··················<0.10
Mn·················0.05—0.20
Mg···············4.50—5.50
Cr················· 0.05—0.20
Zn·················· <0.10
Be··············· <0.0003
Ti················ 0.06—0.20
其余Others···············<0.05
其余總和Others Total··········<0.15
物理性能指標(biāo):
屈服極限 0.2% yield strength Rpo2 (Mpa)··· 110
拉伸強(qiáng)度 Tensile Strength Rm (Mpa)·····240
延伸率 Elongation A5 (L0=5d0) (%)····· 17
試驗(yàn)溫度 Test Temperature (℃)····· 20
性能特點(diǎn)及用途:本品為含鎂5%的鋁合金焊絲,是一種用途廣泛的通用型焊材,適合焊接或堆焊5%鎂的鑄鍛鋁合金,強(qiáng)度高,可鍛性好,抗腐蝕性好。本品能為經(jīng)陽(yáng)極化處理的焊接提供良好的配色。
保護(hù)氣體:焊接氬氣、氮?dú)?、或氬氣—氮?dú)饣旌蠚怏w
規(guī)格Φ
盤(pán)裝焊絲(mm):0.8 ; 0.9 ; 1.0 ; 1.2 ; 1.6 ; 2.0 ; 2.4
直條焊絲(mm):1.6 ; 2.0 ; 2.4 ; 3.2 ; 4.0 ; 5.0 ; 6.0
焊絲的包裝
盤(pán)裝焊絲 :S100/0.5kg 1Lb , S200/2kg , S270-S300/6kg-7kg
直條焊絲 :5/10kg ····長(zhǎng)度 :1000mm